Typical Composition of all-weld Metal
Mechanical Test of weld Metal
- Tempered, 690 oC /1h/furnace up to 300 oC/air.
Operating Data
Re – drying: if necessary: 300 – 350 ºC, min. 2 h.
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description E9018-B3H4R is preferred for 10 CrMo9 10, it has an advantage for items operating under temperature up to 600 °C , ideal for high creep resistance of boilers and pipe lines of the ancillaries of furnaces and heat exchangers. Crack resistance, tough weld metal, high creep strength, weld metal can be nitrided, quenching and tempering. |
| C | Si | Mn | Mo | P | S | Cr | |
| Wt. % | 0.07 | 0.22 | 0.47 | 0.99 | 0.01 | 0.02 | 2.25 |
| Typical According to ASME II part C/SFA 5.5 | 0.05-0.12 | 0.80 max. | 0.90 max. | 0.4-0.65
|
0.03 max. | 0.03 max. | 1.0-1.5 |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | |
| MPa | MPa | % | +20oC | -20 oC | |
| 480 | 570 | 25 | 140 | 65 | |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 530 | ≥ 620 | ≥ 17 | N.S |
Re – drying: if necessary: 300 – 350 ºC, min. 2 h.
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 80-110 | 110 – 145 | 130-190 | 160-230 |