Typical Composition of all-weld Metal
Mechanical Test of weld Metal
- Soundness (x-ray) OK
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description Basic Mn-Mo alloyed electrode especially suited for high-strength fine-grained constructional steels and high-temperature steels, e.g., 15NiCuMoNb5S. Crack resistant, tough and ageing resistant. Excellent weld ability in all positions except vertical-down. Base Materials High-strength fine-grained steels, rail steels up to R 200 (for cladding). |
| C | Si | Mn | P | S | Ni | Mo | |
| Wt. % | 0.052 | 0.40 | 1.23 | 0.02 | 0.02 | 0.59 | 0.36 |
| Typical According to ASME II part C/SFA 5.5 | 0.12 max. | 0.8 max. | 1.0-1.75 | 0.03 max. | 0.03 max. | 0.9 max. | 0.25-0.45 |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | ||
| MPa | MPa | % | +20 oC | |||
| Untreated | 570 | 670 | 22 | 55 | 57 | 54 |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 530 | ≥ 620 | ≥ 17 | ≥ 27 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 70-100 | 110 – 140 | 140-180 | 180-240 |