Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description Rutile electrode suited for corrosion resistant, CrNiMo (N)-steels. Suitable for service temperatures from -60 to +300°C. The weld metal exhibits resistance against pitting corrosion and intergranular corrosion resistance up to 300°C. Good operating characteristics on AC and DC, minimum spatter formation, self-releasing slag with smooth and clean bead surface. |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.02 | 0.70 | 0.9 | 0.01 | 0.02 | 13.0 | 19.2 | 3.7 | 0.02 |
| Typical according to ASME II part C /SFA 5.4 | 0.04 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 12-14 | 18-21 | 3-4 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” -+20 º C |
Ferrite Number |
| Typical | 460 | 610 | 35 | 65 | 8 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 520 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |