Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description The core wire is low carbon alloyed austenitic with basic coating. For application in all branches of steel fabrication ,where same-type steels, including higher- carbon steels and ferritic 13% chrome steels are welded, the weld metals has high toughness, it is applicable for cryogenic down to -196°C. It has good resistance towards the intergranular corrosion UP TO 400 °C. |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.02 | 0.30 | 1.14 | 0.01 | 0.01 | 11.4 | 18.2 | 2.65 | 0.04 |
| Typical according to ASME II part C /SFA 5.4 | 0.04 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 11-14 | 17-20 | 2-3 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule”-50º C |
Ferrite Number |
| Typical | 467 | 622 | 52 | 65 | 4 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 490 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |