Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description Low carbon austenitic rutile- basic electrode. High crack resistance with hard toweld materials, austenite – ferrite joints and weld cladding is achieved through the increased ferrite content in the weld metal, particularly good fine welding properties and excellent AC weldability characterize this product , for operating temperatures up to + 300 °C, for the first layer of weld cladding up to +400 °C. |
| C | Si | Mn | P | S | Ni | Cr | Mo | V | |
| Wt. % | 0.02 | 0.70 | 0.8 | 0.02 | 0.02 | 12.5 | 23.5 | 2.50 | 0.1 |
| Typical according to ASME II part C /SFA 5.4 | 0.04 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 12.14 | 22.25 | 2.0-3.0 | 0.1-0.3 |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact values In J CVN |
||
| MPa | MPa | % | -50 ºC | |||
| Typical | 508 | 710 | 31 | 74 | 72 | 73 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 520 | ≥ 30 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 40-70 | 60-100 | 100-140 | 140-180 |