Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description Basic covered NiCrMo alloyed electrode. Low H2-content ≤5 ml/100 g (HD) in the weld metal; very low moisture pickup during long term storage. For high strength fine grained structural steels, for cast steel qualities; weld metal insensitive to cold cracking. Redry = for 2 h at 300 – 350 °C . |
| C | Si | Mn | P | S | Ni | Mo | |
| Wt. % | 0.09 | 0.30 | 1.28 | 0.02 | 0.02 | 3.02 | 0.4 |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | ||
| MPa | MPa | % | +20 oC | -50 oC | ||
| Untreated | 690 | 770 | 18 | 120 | 55 | |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 670 | ≥ 760 | ≥ 15 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 70-100 | 90-140 | 140-190 | 180-250 |