Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Deposition efficiency 115 %
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description It is basic Ni-alloyed electrode with an excellent mechanical properties, particularly high toughness and crack resistance for higher strength fine-grained constructional steels. It is suitable for service at – 60 ºC to + 350 ºC. Very good impact strength in aged condition. The metal recovery is about 115 %, easily weldable in all positions except vertical – down and very low hydrogen content. |
| C | Si | Mn | P | S | Ni | Cr | Mo | V | |
| Wt. % | 0.07 | 0.58 | 1.00 | 0.02 | 0.02 | 1.05 | 0.02 | 0.32 | 0.02 |
| Typical According to ASME II part C/SFA 5.5 | 0.12 max. | 0.8 max. | 0.4-1.25 | 0.03 max. | 0.03 max. | 0.8-1.1 | 0.15 max. | 0.35 max. | 0.05 max. |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | |
| MPa | MPa | % | -50 oC | ||
| Untreated | 512 | 620 | 27 | 78 | |
| Average Reference According to ASME II part C/SFA 5.5 | 470 – 550 | ≥ 550 | ≥ 24 | ≥ 27 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 80-110 | 100-140 | 130-180 | 180 -230 |