Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description Basic Cr-Mo-Ni-V-W-Nb alloyed electrode suited for welding of high temperature steel 9%Cr-1.5% W-Mo-Nb-N (NF 616, P 92). Approved in long-term condition up to +650 °C service temperature. The electrode features a stable arc, good striking and re-striking properties, low spatter loss and an easy removable slag. |
| C | Si | Mn | P | S | Ni | |
| Wt. % | 0.04 | 0.90 | 1.2 | 0.01 | 0.02 | 1.1 |
| Typical According to ASME II part C/SFA 5.5 | —- | 0.8 min. | 1.0 min. | 0.03 max. | 0.03 max. | 0.5 min. |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | |
| MPa | MPa | % | +30 oC | -40 oC | |
| Untreated | 624 | 720 | 24 | 105 | 92 |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 530 | ≥ 620 | ≥ 17 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5 mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350/450 | 350/450 | 350/450 |
| Amps A | 70-100 | 100-145 | 140-190 | 160-240 |