Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h . |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Basic covered NiMo alloyed electrode with a weld metal of special metallurgical purity for nuclear reactor construction. Quality controlled according to KTA 1408.2; very low H2-content ≤5 ml/100 g; NDT-tested. Used preferably for the welding of steels in the construction of nuclear reactors, boiler and pressure vessels; for fine grained structural steels up to S500Q. |
| C | Si | Mn | P | S | Ni | Cr | |
| Wt. % | 0.08 | 0.81 | 1.17 | 0.02 | 0.02 | 0.65 | 0.44 |
| Typical According to ASME II part C/SFA 5.5 | —– | 0.8 min. | 1.0 min. | 0.03 max. | 0.03 max. | 0.5 min. | 0.2 min. |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | ||
| MPa | MPa | % | -40 oC | -50 oC | ||
| Untreated | 620 | 730 | 24 | 120 | 110 | |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 530 | ≥ 620 | ≥ 17 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h . |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 70-100 | 100-150 | 140-200 | 170-250 |