Weld Metal deposit analysis
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description
|
| C | Si | Mn | P | S | Ni | Cr | Cu | |
| Wt. % | 0.1 | 0.60 | 2.3 | 0.02 | 0.02 | 20.5 | 25.5 | 0.02 |
| Typical according to ASME II part C /SFA 5.4 | 0.08-0.20 | 0.75 max | 1.0-2.5 | 0.03 max | 0.03 max | 20-22.5 | 25-28 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” -50 º C |
Ferrite Number | |
| Typical | 530 | 695 | 51 | 80 | 0 | |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 550 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-200 |