Weld metal deposit analysis
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description It is basic Ni-alloyed electrode with an excellent mechanical properties, |
| C | Si | Mn | P | S | Ni | Cr | Mo | V | |
| Wt. % | 0.07 | 0.38 | 1.12 | 0.02 | 0.02 | 0.93 | 0.05 | 0.01 | 0.02 |
| Typical According to ASME II part C/SFA 5.5 | 0.12 max. | 0.8 max. | 0.4-1.25 | 0.03 max. | 0.03 max. | 0.8-1.1 | 0.15 max. | 0.35 max. | 0.05 max. |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | ||
| MPa | MPa | % | -50 oC | |||
| Typical | 512 | 611 | 27 | 81 | 80 | 82 |
| Average Reference According to ASME II part C/SFA 5.5 | 470 – 550 | ≥ 550 | ≥ 24 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 80-110 | 100-140 | 130-180 | 180 -230 |