Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: not allowed |
Welding Positions
- All
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
|
| C | Si | Mn | Mo | P | S | |
| Wt. % | 0.11 | 0.14 | 0.4 | 0.5 | 0.02 | 0.02 |
| Typical According to ASME II part C/SFA 5.5 | 0.12
max. |
0.40
max. |
0.60
max. |
0.4 – 0.65 | 0.03
max. |
0.03
max. |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | |
| MPa | MPa | % | 0 oC | – 20 oC | |
| Untreated | 480 | 550 | 23 | 100 | 85 |
| Typical According to ASME II part C/SFA 5.5 | ≥ 390 | ≥ 490 | ≥ 22 | N.S |
| Re – drying: not allowed |
| 2.5 mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-90 | 80-130 | 120-180 | 160-210 |