Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description |
| C | Si | Mn | P | S | Ni | Mo | |
| Wt. % | 0.12 | 0.40 | 1.75 | 0.01 | 0.01 | 0.5 | 0.36 |
| Typical According to ASME II part C/SFA 5.5 | 0.15 Max. | 0.80 Max. | 1.65-2.0 | 0.03 Max. | 0.03 Max. | 0.9 Max. | 0.25-0.45 |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | ||
| MPa | MPa | % | -50 oC | |||
| Tempered at 620 °C/1h | 630 | 720 | 22 | 54 | 53 | 55 |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 600 | ≥ 690 | ≥ 16 | ≥ 27 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 75-100 | 110 -140 | 150 -190 | 190 -260 |