Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.01 | 0.80 | 0.83 | 0.01 | 0.01 | 8.7 | 23.1 | 2.94 | 0.15 |
| Typical according to ASME II part C /SFA 5.4 | 0.04-max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 8.5-10.5 | 21.5-23.5 | 2.5-3.5 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact values
In J CVN |
||
| MPa | MPa | % | +20 °C | -30 °C | ||
| Untreated | 650 | 820 | 25 | 55 | 41 | |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 690 | ≥ 20 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 50-80 | 70-120 | 90-160 | 150-220 |