Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description This is a high alloyed low carbon electrode designed for welding dissimilar base metals of stainless steel and mild or low- alloy steels. The electrode is suitable to work as buffer layer when overlay welding on mild steels. Providing an 18 Cr 8Ni deposit from the first layer, this electrode is applicable to weld high temperature steels. |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.025 | 0.80 | 0.8 | 0.02 | 0.02 | 12.6 | 23.2 | 0.01 | 0.01 |
| Typical according to ASME II part C /SFA 5.4 | 0.04 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 12-14 | 22-25 | 0.75 max | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” -50 º C |
Ferrite Number |
| Typical | 475 | 670 | 50 | 75 | 15 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 520 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |