Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description |
| C | Si | Mn | P | S | Ni | Cr | Mo | |
| Wt. % | 0.06 | 0.25 | 0.78 | 0.01 | 0.01 | 0.13 | 1.22 | 0.52 |
| Typical According to ASME II part C/SFA 5.5 | 0.05-0.10 | 0.9 Max. | 1.0 Max. | 0.03 Max. | 0.03 Max. | 0.4 Max. | 8.0-10.5 | 0.85-1.20 |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | ||
| MPa | MPa | % | -50 oC | |||
| Tempered at 740 °C/1h | 612 | 740 | 25 | 75 | 76 | 77 |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 460 | ≥ 550 | ≥ 19 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 70-90 | 100-120 | 130-160 | 160-230 |