Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description This electrode is having core wire with 25 Cr 20 Ni for conducting welding of 1.4845/ASTM310S and similar types of high temperature stainless steels it is strongly recommended to decrease the heat input and the interpass temperature to avoid the risk of hot cracking when welding full austenitic steels and nickel base alloys. |
| C | Si | Mn | P | S | Ni | Cr | Cu | |
| Wt. % | 0.11 | 0.70 | 2.0 | 0.02 | 0.02 | 21.0 | 26.2 | 0.02 |
| Typical according to ASME II part C /SFA 5.4 | 0.08-0.20 | 0.75 max | 1.0-2.5 | 0.03 max | 0.03 max | 20-22.5 | 25-28 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” |
||
| Typical | 520 | 688 | 50 | -50 º C | ||
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 550 | ≥ 30 | 75 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |