Typical Composition of all-weld Metal
Deposition efficiency 115 %
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h . |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description Ni-alloy, basic coated stick electrode are for unalloyed and Ni-alloy fine-grained structural steels, tough, crack-resistant weld metal. It is cryogenic down to -80oC, ideal weldability in all positions except for vertical down. Very low hydrogen content (under AWS conditions HD <= 4 ml/100g). |
| C | Si | Mn | P | S | Ni | |
| Wt. % | 0.08 | 0.42 | 1.2 | 0.01 | 0.01 | 2.43 |
| Typical According to ASME II part C/SFA 5.5 | 0.12 max. | 0.80 max. | 1.25 max. | 0.03 max. | 0.03 max. | 2.0-2.75 |
Deposition efficiency 115 %
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | |
| Tempered at 605 oC/1h | MPa | MPa | % | -60 oC | |
| Untreated | 490 | 570 | 30 | 70 | |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 460 | ≥ 550 | ≥ 19 | ≥ 27 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h . |
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 70-100 | 110-140 | 140-180 | 190-230 |