Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h |
– Deposition efficiency 115 %
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description Basic Coated electrode for high temperature steels up to 550 °C high pressure vessel and tube steels, extremely high ductility and cracking resistance. Metal recovery about 115 %, due to alloying elements which transferred from the flux of filler metal to the weld metal. |
| C | Si | Mn | Mo | P | S | |
| Wt. % | 0.07 | 0.35 | 0.80 | 0.45 | 0.01 | 0.01 |
| Typical According to ASME II part C/SFA 5.5 | 0.12 max. | 0.80 max. | 0.90 max. | 0.4-0.65 | 0.03 max. | 0.03 max. |
| Heat Treatment | Yield Strength 0.2% | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN |
| MPa | MPa | % | -50 oC | |
| Untreated | 460 | 550 | 26 | 65 |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 390 | ≥ 490 | ≥ 22 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h |
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 80-110 | 100 – 140 | 130-180 | 190-230 |
– Deposition efficiency 115 %