Typical Composition of all-weld Metal
Mechanical Test of weld Metal
- – Deposition efficiency 115 %
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description Basic coated Stick electrode of high toughness and crack-resistance for high-strength fine-grained structural steels. Cryogenic down to -60°C, and resistant to ageing. Approved for armour plates. Easily handled in all positions except for vertical down. Very low hydrogen content in the weld metal (under AWS conditions HD ≤ 4 ml/100g). |
| C | Si | Mn | P | S | Ni | Cr | Mo | V | |
| Wt. % | 0.065 | 0.53 | 1.17 | 0.01 | 0.01 | 0.82 | 0.01 | 0.01 | 0.01 |
| Typical According to ASME II part C/SFA 5.5 | — | 0.8 min. | 1.00 min. | 0.03 min. | 0.03 min. | 0.50 min. | 0.30 min. | 0.20 min. | 0.10 min. |
| Heat Treatment | Yield Strength | Tensile Strength | Elongation L0=5d0 | Impact values In J CVN | |
| MPa | MPa | % | -50 oC | ||
| Untreated | 504 | 603 | 27 | 85 | |
| Average Reference According to ASME II part C/SFA 5.5 | ≥ 460 | ≥ 550 | ≥ 19 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| 2.5mm | 3.25 mm | 4.0mm | 5.0mm | |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 80-110 | 100-140 | 130-180 | 180 -230 |