Typical Composition of all-weld Metal
Mechanical properties of all-weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
المنطقة الصناعية A1, 10 من رمضان, مصر

99 ش Sebak الشارع
ماريلاند - مصر الجديدة - القاهرة - مصر
+2012 2100 5111
+2010 0885 1811
Description |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.01 | 0.80 | 0.83 | 0.01 | 0.01 | 8.7 | 23.1 | 2.94 | 0.15 |
| Typical according to ASME II part C /SFA 5.4 | 0.04
max |
1.0
max |
0.5-2.5 | 0.04
max |
0.03
max |
8.5-10.5 | 21.5-23.5 | 2.5-3.5 | 0.75
max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact values
In J CVN |
|
| MPa | MPa | % | +20 °C | -30 °C | |
| Typical | 650 | 820 | 25 | 55 | 41 |
| Typical according to ASME II part C /SFA 5.4 | N.S | ≥ 690 | ≥ 20 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 40-75 | 70-120 | 110-150 | 150-200 |