Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description It is core wire alloyed, rutile coated stick electrode for same type, heat resistant rolled such as in annealing shops, hardening shops, steam boiler constructions, and the petrochemical industry. It has smooth seams and easy slag removal. |
| C | Si | Mn | P | S | Ni | Cr | Cu | |
| Wt. % | 0.12 | 0.50 | 2.1 | 0.01 | 0.01 | 21.0 | 26.0 | 0.02 |
| Typical according to ASME II part C /SFA 5.4 | 0.08-0.20 | 0.75 max | 1.0-2.5 | 0.03 max | 0.03 max | 20-22.5 | 25-28 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” -50 º C |
Ferrite Number |
| Typical | 523 | 690 | 52 | 70 | 0 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 550 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |