Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description The bare wire is low carbon alloyed austenite with basic flux coating, applicable for similar welding in wide range industry, this including high carbon steel and ferritic 13% chrome steels are welded , has phenomenal ability to weld root, excellent bridging , and easy removal of slag, high control of the slag and weld pool , high resistance towards the intergranular corrosion. |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.03 | 0.76 | 1.67 | 0.03 | 0.006 | 9.64 | 20.6 | 0.13 | 0.10 |
| Typical according to ASME II part C /SFA 5.4 | 0.04 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 9-11 | 18-21 | 0.75 max | 0.75 max |
| Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” -50º C |
Ferrite Number | |
| Typical | 506 | 634 | 48 | 100 | 5 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 520 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350/450 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |