Typical Composition of all-weld Metal
Mechanical Test of weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description This type of electrode is a chromium Nickel molybdenum high recover electrode for welding 1.4436/ASTM316 type stainless steels the 2D type electrodes provide a metal recovery of about 150% giving a high deposition rate and improved productivity in horizontal butt and overlay welding . |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.02 | 0.80 | 0.8 | 0.02 | 0.02 | 11.7 | 18.0 | 2.6 | 0.02 |
| Typical according to ASME II part C /SFA 5.4 | 0.04 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 11-14 | 17-20 | 2-3 | 0.75 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule”-50º C |
Ferrite Number |
| Typical | 465 | 620 | 51 | ||
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 490 | ≥ 30 | 67 | 6 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |