Typical Composition of all-weld Metal
Mechanical properties of all-weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h |
Welding Positions
- All, except vertical down
Polarity
- AC & DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description high-alloy fully austenitic Cr-Ni-Mo-Cu electrode designed for welding 1.4539/ASTM 904L type steels. It can also be used for welding 1.4404/ASTM 316 components where a ferrite free weld is required, e.g. in cryogenic or non-magnetic applications. The weld metal has a very good impact toughness at low temperatures. To minimize the risk of hot cracking when welding fully austenitic steels, heat input and interpass temperature must be low and there must be as little dilution as possible from the parent metal. |
| C | Si | Mn | P | S | Ni | Cr | Mo | Cu | |
| Wt. % | 0.02 | 0.55 | 1.25 | 0.01 | 0.01 | 25.2 | 20.5 | 4.8 | 1.6 |
| Typical according to ASME II part C /SFA 5.4 | ≤ 0.03 | ≤ 0.09 | 1-2.5 | ≤ 0.03 | ≤ 0.02 | 24-26 | 19.5-21.5 | 4.2-5.2 | 1.2-2 |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule” |
| MPa | MPa | % | – 196 °C | |
| untreated | 410 | 630 | 38 | 55 |
| Typical according to ASME II part C /SFA 5.4 | N.S | ≥ 520 | ≥ 30 | N.S |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350/450 | 350 |
| Amps A | 35-75 | 55-110 | 100-150 | 140-190 |