Typical Composition of all-weld Metal
Mechanical properties of all-weld Metal
Operating Data
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description Due to the presence of Nb it`s stabilized, core wire alloyed austenitic stick electrode with basic coating, the weld metal has high toughness. Cryogenic down to – 196 °C. Resists intergranular corrosion UP TO + 400 °C. |
| C | Si | Mn | P | S | Ni | Cr | Nb | |
| Wt. % | 0.02 | 0.8 | 0.8 | 0.02 | 0.02 | 10.2 | 19.3 | 0.25 |
| Typical according to ASME II part C /SFA 5.4 | 0.08 max | 1.0 max | 0.5-2.5 | 0.04 max | 0.03 max | 9-11 | 18-21 | 1.0 max |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact Strength “Joule”-+20º C |
Ferrite Number |
| Untreated | 480 | 630 | 37 | 54 | 5 |
| Typical According to ASME II part C/SFA 5.4 | N.S | ≥ 520 | ≥ 30 |
| Re – drying: if necessary: 300 – 350 ºC, min. 2 h |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 50-80 | 80-110 | 110-140 | 140-180 |