Typical Composition of all-weld Metal
Mechanical properties of all-weld Metal
Operating Data
| Re – drying : if necessary: 300 – 350 ºC, min. 2 h. |
Welding Positions
- All, except vertical down
Polarity
- DC (+)
Industrial Zone A1, 10th of Ramadan City, Egypt

99 El Sebak Street
Maryland - Heliopolis - Cairo - Egypt
+2012 2100 5111
+2010 0885 1811
Description |
| C | Si | Mn | P | S | Ni | Cr | Mo | |
| Wt. % | 0.03 | 0.58 | 0.80 | 0.01 | 0.01 | 9.3 | 25.4 | 4.2 |
| Typical according to ASME II part C /SFA 5.4 | 0.04
max |
1.0
max |
0.5-2 | 0.04
max |
0.03
max |
8.0-10.5 | 24-27 | 3.5-4.5 |
| Heat
Treatment |
Yield Strength N/mm2 | Tensile Strength N/mm2 | Elongation% L0=5d0 | Impact values
In J CVN |
FN | |
| MPa | MPa | % | +20 °C | -50 °C | ||
| Typical | 680 | 880 | 26 | 75 | 50 | 10 |
| Typical according to ASME II part C /SFA 5.4 | N.S | ≥ 760 | ≥ 15 |
| Re – drying : if necessary: 300 – 350 ºC, min. 2 h. |
| mm | 2.5mm | 3.25 mm | 4.0mm | 5.0mm |
| L mm | 350 | 350 | 350 | 350 |
| Amps A | 40-80 | 75-110 | 100-150 | 130-200 |